Iru | Grage No. | Aifarahan | NV (%) | EEW (g/eq) | Igi iki (mpa.s/25℃) | P% (%) |
DOPO títúnṣe phenolic epoxy resini | EMTE 8202-M75 | Aila-awọ si imọlẹ ofeefee sihin omi | 75± 1.0 | 315±20 | 1000-3000 | 3.1 ~ 3.2 |
DOPO títúnṣe phenolic epoxy resini | EMTE 8202A-K70 | Omi pupa pupa pupa | 70± 1.0 | 300±20 | <2000 | 2.4± 0.1 |
DOPO títúnṣe phenolic epoxy resini | EMTE 3202B-EK75 | Aila-awọ si imọlẹ ofeefee sihin omi | 75± 1.0 | 310±20 | ≤3000 | 2.8 ~ 3.2 |
DOPO títúnṣe phenolic epoxy resini | EMTE 8202C-K75 | Omi mimọ ati sihin | 75± 1.0 | 300±20 | <3000 | 3.1 ± 0.1 |
DOPO títúnṣe phenolic epoxy resini | EMTE 8202D-K75 | Ina ofeefee sihin omi | 70± 1.0 | 360± 30 | ≤1500 | 2.5± 0.2 |
Iru | Grage No. | Aifarahan | NV (%) | EEW (g/eq) | Igi iki (mpa.s/25℃) | P% (%) |
DOPO-HQ títúnṣe phenolic iposii resini | EMTE 8200-K70 | Omi pupa pupa pupa | 70± 1.0 | 320±20 | <1000 | 2.0 ± 0.1 |
DOPO-HQ títúnṣe phenolic iposii resini | EMTE 8200A-K70 | Omi pupa pupa pupa | 70± 1.0 | 275±25 | <1000 | 1.0 ± 0.1 |
DOPO-HQ títúnṣe phenolic iposii resini | EMTE 82300C-M80 | Yellow sihin omi | 80± 1.0 | 255±15 | 1000-7000 | 2.0 ± 0.1 |
DOPO-HQ títúnṣe phenolic iposii resini | EMTE 8200D-MCS80 | Yellow sihin omi | 80± 1.0 | 230±20 | 1000-4000 | 1.0 ± 0.1 |
Iru | Grage No. | Aifarahan | NV (%) | EEW (g/eq) | Igi iki (mpa.s/25℃) | P% (%) |
DOPO-HQ títúnṣe phenolic iposii resini | EMTE 8200-K70 | Omi pupa pupa pupa | 70± 1.0 | 320±20 | <1000 | 2.0 ± 0.1 |
DOPO-HQ títúnṣe phenolic iposii resini | EMTE 8200A-K70 | Omi pupa pupa pupa | 70± 1.0 | 275±25 | <1000 | 1.0 ± 0.1 |
DOPO-HQ títúnṣe phenolic iposii resini | EMTE 82300C-M80 | Yellow sihin omi | 80± 1.0 | 255±15 | 1000-7000 | 2.0 ± 0.1 |
DOPO-HQ títúnṣe phenolic iposii resini | EMTE 8200D-MCS80 | Yellow sihin omi | 80± 1.0 | 230±20 | 1000-4000 | 1.0 ± 0.1 |